A tungsten-carbide insert finishing case targeting roughness below Ra 0.05 µm and edge radius no greater than 5 µm while avoiding cobalt-binder leaching.
| Component | Ground tungsten-carbide inserts |
|---|---|
| Primary risk | Cobalt-binder leaching |
| Finishing process | Dry electropolishing |
| Batch size | 80 pieces |
| Documented process time | 7 minutes |
| Target roughness | Ra < 0.05 µm |
| Maximum controlled edge radius | 5 µm |
| Previous extra grinding time | About 30 minutes per piece |
| Selective protection | Masking can preserve designated areas |
Tungsten carbide is difficult to polish mechanically because aggressive abrasion can round cutting edges. Chemical or conventional electrochemical attack can remove cobalt binder, leaving voids and weakening the structure.
The previous high-end workflow added individual robotic grinding and sharpening with a diamond wheel.
The dry-electropolishing process completed an 80-piece batch in seven minutes. The prior supplemental operation took approximately 30 minutes per piece.
Masking can be applied to prevent treatment of selected surfaces or features.
POLISHX technical profile · 2026-10-13 13:31:12