Struers methods: Carbonitrided Steels Brittle Surface 1942 Susp P Lub. Source classification: Ferrous Metals.

Searchable text transcription
The page images and original PDF preserve the table layout and notation.
Grinding Steps PG FG FG 2 FG 3 Surface Type SiC Foil #320 SiC Foil #500 SiC Foil #1200 MD-Largo Disc speed (rpm) 300 300 300 150 Abrasive Type DP-Susp. P 9 µm Predosing/dosing 3/6 Lubricant Type Water Water Water DP-Blue Predosing/dosing 3/6 Force (N) 30 30 30 30 Holder direction >> >> >> >> Holder speed (rpm) 150 150 150 150 Time (min) 1 1 1 7 Carbonitrided Steels - Brittle surface 1942 Ferrous Metals Susp. P/Lub. Polishing Steps DP DP 2 Surface Type MD-Dac MD-Nap Disc speed (rpm) 150 150 Abrasive Type DP-Susp. P 3 µm DP-Susp. P 1 µm Predosing/dosing 3/6 3/6 Lubricant Type DP-Blue DP-Blue Predosing/dosing 3/10 3/14 Force (N) 30 20 Holder direction >> >> Holder speed (rpm) 150 150 Time (min) 5 2 The method is developed to fit a standard equipment configuration with 30 mm specimen on 300mm disc. Dosing levels are valid for following equipment: Tegramin, AbraPol and LaboPol For advice on how to adjust the method to fit your equipment, please take a look at Preparation Parameters. The preparation time for the plane grinding (PG) step depends very much on the condition of the samples and if they are prepared as single specimens or clamped in a specimen holder. Please check the samples after the first step and repeat it if necessary. Method comments Take a look at Preparation Parameters